Access the full text.
Sign up today, get DeepDyve free for 14 days.
AK Lakshminarayanan, K Shanmugam, V Balasubramanian (2009)
Effect of welding processes on tensile and impact properties, hardness and microstructure of AISI 409 M ferritic stainless joints fabricated by duplex stainless steel filler metalJ Iron Steel Res Int, 16
ZH Xie (2011)
Efforts to achieve new breakthroughs in the development of remanufacturing industryChina Surf Eng, 24
WG Xu, FM Burdekin (1998)
Effects of residual stresses on constraint and fracture behavior of wide platesMath Phys Eng Sci, 454
WX Wang, LX Huo, YF Zhang (2002)
Investigation on phase stress and its application to improving fatigue strength of welding jointsChin J Mech Eng, 38
WD Zhang, JB Cui (2005)
Repairing instances with manual arc resurfacing weldingEquip Technol, 2
X Sun (2008)
The repair of final axle shaft threads of TY320 bulldozerOper Maint, 39
J Hou, QJ Peng, Y Takeda (2010)
Microstructure and mechanical property of the fusion boundary region in an alloy 182-low alloy steel dissimilar weld jointJ Mater Sci, 45
BS Xu (2010)
Recent progress of remanufacture industry and technology in ChinaTherm Spray Technol, 2
ZW Tang (2007)
Exploration of repair methods for driving axle housing of Dongfeng dump truckAuto Maint Repair, 11
Screw failure is one of the main scrap forms for rear axle tube, and thread turning after surfacing is a common means of remanufacturing. This paper takes rear axle tube as the main research topic, which is made of 40Mn and provided by an axle company. Manual electric arc welding, CO2 shielded arc welding and argon shielded arc welding are carried to overlay the damaged thread. The deposited metal consists of two welding material lays. Welding process and overlay properties are characterized by the test and analysis of microstructure, residual stress and hardness of surfacing layers. The results show that argon shielded arc welding is an effective method to repair the failure thread; its microstructure of fusion area is meticulous and uniform; its residual compressive stress (absolute value) of welding surface is the biggest among the three welding methods; its hardness curve is relatively flat and appropriate for turning.
Advances in Manufacturing – Springer Journals
Published: May 11, 2013
Read and print from thousands of top scholarly journals.
Already have an account? Log in
Bookmark this article. You can see your Bookmarks on your DeepDyve Library.
To save an article, log in first, or sign up for a DeepDyve account if you don’t already have one.
Copy and paste the desired citation format or use the link below to download a file formatted for EndNote
Access the full text.
Sign up today, get DeepDyve free for 14 days.
All DeepDyve websites use cookies to improve your online experience. They were placed on your computer when you launched this website. You can change your cookie settings through your browser.