Enhancement of the punch pin durability induced by the PVD coating in production process of the automotive inner pipe

Enhancement of the punch pin durability induced by the PVD coating in production process of the... This experimental studies were carried out in order to understand the effects of the PVD coating and the UNSM treatment of HSS55 (high speed steel 55) during the production of the automotive inner pipe by the plastic deformation of S45C. The field test and the SEM images revealed that the PVD coating is necessary in spite of the high compressive residual stresses which were formed at the head of a punch pin. Upon the application of the AlCrN coating with the UNSM treatment the productivity and reliability of a punch pin had improved more than about 2.6 times compared to that of the TiN coating without the UNSM treatment. It is likely that the improvement is caused by the decreased stress concentration factor by the ‘wrapped in oxides’ inside of an abrasion pit. The abrasion pits were mostly generated within range of 5% ∼ 50% of the diameter ratio from the end of a pin and reached the maximum value about 17% from the end of a pin. http://www.deepdyve.com/assets/images/DeepDyve-Logo-lg.png Journal of Mechanical Science and Technology Springer Journals

Enhancement of the punch pin durability induced by the PVD coating in production process of the automotive inner pipe

Loading next page...
 
/lp/springer-journals/enhancement-of-the-punch-pin-durability-induced-by-the-pvd-coating-in-4SZHq5YC0u

References (12)

Publisher
Springer Journals
Copyright
Copyright © 2010 by The Korean Society of Mechanical Engineers and Springer-Verlag Berlin Heidelberg
Subject
Engineering; Industrial and Production Engineering; Vibration, Dynamical Systems, Control; Mechanical Engineering
ISSN
1738-494X
eISSN
1976-3824
DOI
10.1007/s12206-010-0314-7
Publisher site
See Article on Publisher Site

Abstract

This experimental studies were carried out in order to understand the effects of the PVD coating and the UNSM treatment of HSS55 (high speed steel 55) during the production of the automotive inner pipe by the plastic deformation of S45C. The field test and the SEM images revealed that the PVD coating is necessary in spite of the high compressive residual stresses which were formed at the head of a punch pin. Upon the application of the AlCrN coating with the UNSM treatment the productivity and reliability of a punch pin had improved more than about 2.6 times compared to that of the TiN coating without the UNSM treatment. It is likely that the improvement is caused by the decreased stress concentration factor by the ‘wrapped in oxides’ inside of an abrasion pit. The abrasion pits were mostly generated within range of 5% ∼ 50% of the diameter ratio from the end of a pin and reached the maximum value about 17% from the end of a pin.