Get 20M+ Full-Text Papers For Less Than $1.50/day. Start a 14-Day Trial for You or Your Team.

Learn More →

A Treatise on Corrosion Science, Engineering and TechnologyMitigating Environmentally Assisted Cracking in 7xxx Cu Containing Aluminum Alloys

A Treatise on Corrosion Science, Engineering and Technology: Mitigating Environmentally Assisted... [Environmentally assisted cracking in high strength 7xxx Cu containing aluminum alloys has been a prevalent problem for a significantly long time. Several advancements in alloy chemistry and processing techniques (heat treatments) have led to marked improvements in the resistance of these alloys to environmentally assisted cracking. This chapter provides a brief account of various heat treatments, their limitations, and the underlying metallurgical factors that led to various developments in mitigating environmentally assisted cracking.] http://www.deepdyve.com/assets/images/DeepDyve-Logo-lg.png

A Treatise on Corrosion Science, Engineering and TechnologyMitigating Environmentally Assisted Cracking in 7xxx Cu Containing Aluminum Alloys

Part of the Indian Institute of Metals Series Book Series
Editors: Kamachi Mudali, U.; Subba Rao, Toleti; Ningshen, S.; G. Pillai, Radhakrishna; P. George, Rani; Sridhar, T. M.

Loading next page...
 
/lp/springer-journals/a-treatise-on-corrosion-science-engineering-and-technology-mitigating-R0SzJJqtyK

References (0)

References for this paper are not available at this time. We will be adding them shortly, thank you for your patience.

Publisher
Springer Nature Singapore
Copyright
© The Editor(s) (if applicable) and The Author(s), under exclusive license to Springer Nature Singapore Pte Ltd. 2022
ISBN
978-981-16-9301-4
Pages
223 –236
DOI
10.1007/978-981-16-9302-1_13
Publisher site
See Chapter on Publisher Site

Abstract

[Environmentally assisted cracking in high strength 7xxx Cu containing aluminum alloys has been a prevalent problem for a significantly long time. Several advancements in alloy chemistry and processing techniques (heat treatments) have led to marked improvements in the resistance of these alloys to environmentally assisted cracking. This chapter provides a brief account of various heat treatments, their limitations, and the underlying metallurgical factors that led to various developments in mitigating environmentally assisted cracking.]