Shyam Lal, Sudhir Kumar, Z. Khan, A. Siddiquee (2015)
Multi-response optimization of wire electrical discharge machining process parameters for Al7075/Al2O3/SiC hybrid composite using Taguchi-based grey relational analysisProceedings of the Institution of Mechanical Engineers, Part B: Journal of Engineering Manufacture, 229
Wang Zhenlong, Geng Xuesong, Chi Guanxin, Wang Yukui (2014)
Surface Integrity Associated with SiC/Al Particulate Composite by Micro-Wire Electrical Discharge MachiningMaterials and Manufacturing Processes, 29
R. Khanna, N. Sharma, Nilesh Kumar, R. Gupta, Abhishek Sharma (2022)
WEDM of Al/SiC/Ti composite: A Hybrid Approach of RSM-ARAS-TLBO AlgorithmInternational Journal of Lightweight Materials and Manufacture
Akash Nag, A. Srivastava, A. Dixit, A. Mandal, A. Das, Tanmay Tiwari (2018)
Surface Integrity analysis of Wire-EDM on in-situ hybrid composite A359/Al2O3/B4CMaterials Today: Proceedings, 5
M. Krishna, Anthony Xavior (2014)
An Investigation on the Mechanical Properties of Hybrid Metal Matrix CompositesProcedia Engineering, 97
Anish Kumar, Vinod Kumar, J. Kumar (2016)
Surface crack density and recast layer thickness analysis in WEDM process through response surface methodologyMachining Science and Technology, 20
P. Abhilash, D. Chakradhar (2021)
Machine-vision-based electrode wear analysis for closed loop wire EDM process controlAdvances in Manufacturing, 10
A. Puri, B. Bhattacharyya (2005)
Modeling and analysis of white layer depth in a wire-cut EDM process through response surface methodologyThe International Journal of Advanced Manufacturing Technology, 25
M. Sijo, K. Jayadevan (2016)
Analysis of Stir Cast Aluminium Silicon Carbide Metal Matrix Composite: A Comprehensive Review☆Procedia Technology, 24
Himanshu Kala, K. Mer, Sandeep Kumar (2014)
A Review on Mechanical and Tribological Behaviors of Stir Cast Aluminum Matrix Composites.Procedia Materials Science, 6
Anish Kumar, Vinod Kumar, J. Kumar (2014)
MICROSTRUCTURE ANALYSIS AND MATERIAL TRANSFORMATION OF PURE TITANIUM AND TOOL WEAR SURFACE AFTER WIRE ELECTRIC DISCHARGE MACHINING PROCESSMachining Science and Technology, 18
Anish Kumar, Vinod Kumar, J. Kumar (2013)
Investigation of machining parameters and surface integrity in wire electric discharge machining of pure titaniumProceedings of the Institution of Mechanical Engineers, Part B: Journal of Engineering Manufacture, 227
T. Mythili, R. Thanigaivelan (2020)
Optimization of wire EDM process parameters on Al6061/Al2O3 composite and its surface integrity studies
J. Liu, Lejing Li, Yuebin Guo (2014)
Surface integrity evolution from main cut mode to finish trim cut mode in W-EDM of shape memory alloyApplied Surface Science, 308
K. Jangra (2015)
An experimental study for multi-pass cutting operation in wire electrical discharge machining of WC-5.3% Co compositeThe International Journal of Advanced Manufacturing Technology, 76
L. Li, Yuebin Guo, X. Wei, W. Li (2013)
Surface Integrity Characteristics in Wire-EDM of Inconel 718 at Different Discharge EnergyProcedia CIRP, 6
Vijender Singh, Kamal Kumar, Puneet Katyal (2020)
Experimental Investigation on Surface Integrity and Wear Behavior of Ti-6Al-7Nb Alloy under Rough and Trim Cut Modes of Wire Electrical Discharge MachiningJournal of Materials Engineering and Performance, 30
S. James, K. Venkatesan, P. Kuppan, R. Ramanujam (2014)
Hybrid Aluminium Metal Matrix Composite Reinforced with SiC and TiB2Procedia Engineering, 97
Amit Goswami, J. Kumar (2014)
Investigation of surface integrity, material removal rate and wire wear ratio for WEDM of Nimonic 80A alloy using GRA and Taguchi methodEngineering Science and Technology, an International Journal, 17
Fabian Kneubühler, M. Wiessner, K. Wegener (2020)
Analysis of WEDM Process with Respect to Wire Wear and Wire ConsumptionProcedia CIRP, 95
T. Singh, J. Kumar, J. Misra (2022)
Surface integrity analysis of machined surface of Ni-Ti shape memory alloy during wire spark erosion machiningAircraft Engineering and Aerospace Technology
J. Gamage, A. DeSilva (2016)
Effect of Wire Breakage on the Process Energy Utilisation of EDMProcedia CIRP, 42
Harmesh Kumar, Rajesh Kumar, A. Manna, Amresh Kumar (2022)
Analysis of wire electrode wear ratio during WEDM of Al-metal matrix compositeMaterials Today: Proceedings
A. Kumar, V. Kumar, J. Kumar (2013)
Investigation of machining parameters and surface integrity in wire electric discharge machining of pure titaniumProc IMechE Part B: J Engineering Manufacture, 227
S. Rahman, Md. Ashraf, M. Bashar, M. Kamruzzaman, A. Amin, M. Hossain (2017)
Crystallinity, surface morphology, and chemical composition of the recast layer and rutile-TiO2 formation on Ti-6Al-4V ELI by wire-EDM to enhance biocompatibilityThe International Journal of Advanced Manufacturing Technology, 93
Nilesh Kumar, Jatinder Kumar (2023)
Investigation of machining characteristics and surface integrity for trim cut WEDM of hybrid metal matrix composite [Al 6061, SiC, and TiB2]Journal of Engineering and Applied Science, 70
Thrinadh Jadam, S. Datta, M. Masanta (2019)
Study of surface integrity and machining performance during main/rough cut and trim/finish cut mode of WEDM on Ti–6Al–4V: effects of wire materialJournal of the Brazilian Society of Mechanical Sciences and Engineering, 41
The purpose of this paper is to investigate the surface integrity features, including surface roughness (SR), recast layer (RL), material migration, topography and wire wear pattern in rough and trim-cut wire electric discharge machine (WEDM) of hybrid composite (Al6061-90%/SiC-2.5%/TiB2-7.5%).Design/methodology/approachEffects of four important factors, namely, rough-cut history (RCH), pulse on time (Ton), peak current (IP) and wire offset (WO) have been assessed on the responses of interest for trim-cut WEDM. Box–Behnken design (RSM) was used to formulate the experimentation plan. Quantitative indices of surface integrity, namely, SR and RL, and selected samples have been investigated for qualitative analysis, namely, surface topography, material migration and wire wear pattern.FindingsTon and IP are found to be most significant, whereas RCH and WO are found insignificant for SR. Ton and WO were found to be the most significant factors affecting RL. After trim cut, an RL of thickness 8.26 µm is observed if the initial rough cut has been accomplished at high discharge energy setting. Whereas the best value of RL thickness, i.e. 5.36 µm, can be realized with low level of RCH. A significant decrease in the presence of foreign materials is recorded, indicating its strong correlation with the discharge energy used during machining.Originality/valueInvestigation on surface integrity features for machining of hybrid composite through rough and trim-cut WEDM has been reported by only a limited number of researchers in the past. This study is attempted at fulfilling few vital gaps by addressing the issues such as evaluation of the efficacy of trim cutting under different discharge energy conditions (using RCH), analysis of wire wear pattern in both rough and trim-cut modes and investigation of the wire breakage phenomenon during machining.
Aircraft Engineering and Aerospace Technology: An International Journal – Emerald Publishing
Published: Sep 30, 2024
Keywords: Hybrid MMC; Trim cutting; WEDM; SEM mapping; Surface integrity; Wire wear
Read and print from thousands of top scholarly journals.
Already have an account? Log in
Bookmark this article. You can see your Bookmarks on your DeepDyve Library.
To save an article, log in first, or sign up for a DeepDyve account if you don’t already have one.
Copy and paste the desired citation format or use the link below to download a file formatted for EndNote
Access the full text.
Sign up today, get DeepDyve free for 14 days.
All DeepDyve websites use cookies to improve your online experience. They were placed on your computer when you launched this website. You can change your cookie settings through your browser.