% loading of 300-μm filler in comparison to filler of 425 and 600 μm. The tensile strength of pure vinyl ester showed 65 MPa, and it increased to 99 MPa for 20% filler of 300-μm size. Similar observation ...
or mats) on the mechanical characteristics of the sandwich structures. Specimens were subjected to flexural, flatwise and edgewise compression , and Shore-D hardness testing. General comparison between ...
tested for mechanical properties ( tensile strength, elongation, Young’s modulus, maximum load at yield and flexural test). The last test was about analysing DMA characteristics . SEM images of the fracture ...