Pitting corrosion behaviour of austenitic stainless steels – combining effects of Mn and Mo additions

Pitting corrosion behaviour of austenitic stainless steels – combining effects of Mn and Mo... http://www.deepdyve.com/assets/images/DeepDyve-Logo-lg.png Corrosion Science CrossRef

Pitting corrosion behaviour of austenitic stainless steels – combining effects of Mn and Mo additions

Corrosion Science , Volume 50 (6): 1796-1806 – Jun 1, 2008